Product |
Polyester putty |
Scrape Method |
1.Get the substrate sanded and cleaned. 2.Mix the putty with hardener, the mixing ratio is 100:2-3. 3.Apply smooth film immediately after mixing, avoiding air entrapment. |
Port life |
9-13 minutes. |
Sanding time |
30-40 minutes@25℃. |
Sanding |
Coarse sand P80-P120, Final sand P180-P240. |
Substrate |
Steel, primer and old paint film. |
Unapplicable |
Corroded steel, galvanized steel. |